I have a makeshift gasket made out of sheet metal on both the petcock and fuel gauge sender hole. In about 2 hours I'm removing the acid, drying, and then dumping in the por15 fuel sealer.
Any idea on how long it takes to harden? My thought is that I'll need to remove the gaskets so I can ensure I still have a fuel gauge sender and petcock hole.
Dont want the sealer hardening over it.... any recommendations on whether to wait for it to harden and then carve away at it, or remove the gaskets relatively quickly (right after ensuring all surfaces are coated) so it doesnt harden to begin with.Thanks in advance!
secondary question
They strongly recommended using their other products (metal ready and something else) because they said it wont adhere at all to phosphoric acid.... (i assume this is why Nessism recommended i break up all the phosphate left behind with aquarium rocks) Anyone else have any advice on this?